PHYSICAL PROPERTIES
|
|
Nominal Gauge
Gauge Tolerance (+-%)
Yield (in2/lb)
|
1.38 mil
8 - 10
21,739
|
|
Property |
Typical Value (1) |
Unit |
Test Method |
Haze |
9.1 |
% |
ASTM D 1003 |
COF |
0.29 |
|
ASTM D 1894 |
Dart Impact (F50) |
172 |
Grams |
ASTM D 1709 |
Elmendorf MD Tear |
372 |
Grams |
ASTM D 1922 |
TD Tear |
916 |
Grams |
|
MD Elongation |
546 |
% |
ASTM D822 |
MD Break Energy |
2.15 |
ft-lb. |
ASTM D822 |
TD Elongation |
602 |
% |
ASTM D822 |
TD Break Energy |
2.15 |
ft-lb. |
ASTM D822 |
|
|
- Typical values represent average laboratory values and are intended as guides only, not as specifications.
- Film properties are typical of blown film extruded at approximately a 2.5:1 blowup ratio.
- Properties designated have been determined in accordance with the current issues of the specified test methods.
|
|
|
|
- A higher strength, low slip film designed for use in a multiple of applications. Manufactured from prime Octene polyethylene resins, this film can be engineered with additive packages to suit a variety of applications. Exceptional toughness and machinability.
|